Enabling a highly reversible conversion reaction in a lithiated nano-SnO2 film coated with Al2O3 by atomic layer deposition

This paper was not found in any repository, but could be made available legally by the author.
This paper was not found in any repository, but could be made available legally by the author.

Full text: Unavailable

Green circle
Preprint: archiving allowed
Orange circle
Postprint: archiving restricted
Red circle
Published version: archiving forbidden
Data provided by SHERPA/RoMEO

Abstract

The Al2O3 coating helped to increase the boundary integrity of SnO2 nanocrystals to prevent the lithiation-induced Sn coarsening during cycling, ensuring a highly reversible conversion reaction.