Royal Society of Chemistry, Catalysis Science & Technology, 20(11), p. 6724-6731, 2021
DOI: 10.1039/d1cy00941a
Full text: Unavailable
Remote photocatalytic graphite oxidation proceeds efficiently via a transparent titania photocatalyst thin film coating activating the surface with oxygen functional groups.