Published in

Royal Society of Chemistry, Journal of Materials Chemistry A: materials for energy and sustainability, 11(9), p. 6790-6796, 2021

DOI: 10.1039/d0ta11457j

Links

Tools

Export citation

Search in Google Scholar

Dual active sites fabricated through atomic layer deposition of TiO2 on MoS2 nanosheet arrays for highly efficient electroreduction of CO2 to ethanol

This paper was not found in any repository, but could be made available legally by the author.
This paper was not found in any repository, but could be made available legally by the author.

Full text: Unavailable

Green circle
Preprint: archiving allowed
Orange circle
Postprint: archiving restricted
Red circle
Published version: archiving forbidden
Data provided by SHERPA/RoMEO

Abstract

Ultrathin TiO2/MoS2 nanosheet arrays containing dual active sites could achieve efficient CO2 reduction reaction toward ethanol. A new regulatory mechanism of the CO coupling reaction was proposed based on experimental results and DFT calculations.