Royal Society of Chemistry, Nanoscale, 16(12), p. 9005-9013, 2020
DOI: 10.1039/d0nr01092h
Full text: Unavailable
Thermal atomic layer deposition of Au nanoparticles on titania in a fluidized bed reactor. Effects of precursor pulse time on Au nanoparticle size and loading.