Royal Society of Chemistry, Energy & Environmental Science, 3(13), p. 958-967, 2020
DOI: 10.1039/c9ee04020j
Full text: Unavailable
A 14.57% PCE is achieved in optimized ternary OSCs with 300 nm active layers compatible with R2R large-scale printing process, indicating that thick-film ternary strategy has great potential in achieving efficient large-scale OSCs.