Effect of Strain Rate on Deformation Behavior of AlCoCrFeNi High-Entropy Alloy by Nanoindentation

Journal article published in 2016 by L. Tian, Z. M. Jiao, G. Z. Yuan, S. G. Ma, Z. H. Wang, H. J. Yang, Y. Zhang ORCID, J. W. Qiao