Trans Tech Publications, Materials Science Forum, (844), p. 3-6
DOI: 10.4028/www.scientific.net/msf.844.3
Full text: Unavailable
The thermal barrier coating that consisted of ZrO2-8Y2O3 top-coat and Ni-22Cr-10Al-1Y bond-coat corroded in Ar-1%SO2 gas at 1000-1200°C for up to 300 h. The top-coat and bond-coat consisted primarily of β-ZrO2 and (γ-Ni, α-Al2O3), respectively. During corrosion, Al oxidized preferentially to α-Al2O3 to protect TBC, and sulfidation occurred to a small extent.