Published in

Materials Research Society, Materials Research Society Symposium Proceedings, (1001), 2007

DOI: 10.1557/proc-1001-m05-03

Links

Tools

Export citation

Search in Google Scholar

Influence of Thermal Treatment on YBa2Cu3O7-x Thick Films Prepared by Electrophoretic Deposition on Ni and Ag Substrates

This paper was not found in any repository, but could be made available legally by the author.
This paper was not found in any repository, but could be made available legally by the author.

Full text: Unavailable

Red circle
Preprint: archiving forbidden
Green circle
Postprint: archiving allowed
Green circle
Published version: archiving allowed
Data provided by SHERPA/RoMEO

Abstract

AbstractWe have studied the sintering parameters of YBa2Cu3O7-x (YBCO) coatings produced by electrophoretic deposition (EPD) on Ag and Ni substrates. The maximal sintering temperature is ∼ 930°C due to partial melting and chemical contamination for Ag and Ni substrates respectively. Increasing the sintering duration does not improve significantly the densification. When Ar sintering atmosphere is used, the coating density is strongly increased on Ag substrates while adhesion is poor on Ni substrates. The Ar-sintered YBCO coating deposited on planar Ag substrate displays a significant magnetic shielding effect for low frequency applied magnetic induction.