Laboratory measurements have been made of the thermal conductivity and diffusivity of four rock salts, two anhydrites, and two dolomites bordering the Cycle 4 and Cycle 5 bedded salt formations in the Permian Basin in Deaf Smith County, Texas. Measurement conditions ranged from 303 to 473 K in temperature, and 0.1 to 31.0 MPa in hydrostatic confining pressure. Within the +-5% measurement resolution neither conductivity nor diffusivity showed a dependence upon pressure in any of the rocks. Conductivity and diffusivity in all rocks had a negative temperature dependence. For the two Cycle 4 salt samples, conductivity over the temperature range explored fell from 5.5 to 3.75 W/m.K, and diffusivity fell from about 2.7 to 1.7 x 10/sup -6/ m/sup 2//s. One of the Cycle 5 salts was a single crystal which had anomalous results, but the other had a low conductivity, about 3.4 W/m.K, with very weak temperature dependence, and a high diffusivity, 3.8 to 2.5 x 10/sup -6/ m/sup 2//s over the temperature range. In the nonsalts, conductivity and diffusivity decreased 10 to 20% over the temperature range explored, which was 308