Electro-oxidation of glycerol at Pd based nano-catalysts for an application in alkaline fuel cells for chemicals and energy cogeneration

Journal article published in 2010 by Mário Simões ORCID, Stève Baranton, Christophe Coutanceau
This paper was not found in any repository, but could be made available legally by the author.
This paper was not found in any repository, but could be made available legally by the author.

Full text: Unavailable

Green circle
Preprint: archiving allowed
Red circle
Postprint: archiving forbidden
Red circle
Published version: archiving forbidden
Data provided by SHERPA/RoMEO

Abstract

Carbon supported Pd, Pt, Au and bimetallic PdAu and PdNi nano-catalysts with different compositions were synthesized. Their catalytic activity toward glycerol electro-oxidation was evaluated in alkaline medium. Physical and electrochemical methods where used to characterize the structure and the surface of the catalysts. It was shown that the Pd(x)Au(1-x)/C catalysts were alloys, which present an increase of crystallite (XRD) and particle (TEM) sizes with increasing Au atomic fraction. Their surfaces were palladium rich whatever the Pd atomic ratio. The structure of the Pd(0.5)Ni(0.5)/C catalyst is much more difficult to understand, but it seems to be composed of a palladium phase in interaction with a Ni(OH)(2) phase. The onset potential of glycerol oxidation is ca. 0.15 V lower on Pt/C than on Pd/C and Au/C. All Pd(x)Me(1-x)/C catalysts presented lower onset potential than monometallic Au/C and Pd/C ones, but higher than Pt/C. For bimetallic catalysts, the order of activity at low potentials is: Pd(0.3)Au(0.7)/C > Pd(0.5)Au(0.5)/C > Pd(0.5)Ni(0.5)/C. Electrochemical experiments and in situ infrared spectroscopy measurements have shown that glycerol electro-oxidation mechanism is dependent on the catalyst, leading to different reaction products. Adsorbed CO species are detected on monometallic Pt and on I'd rich catalysts, but not on Au and Pd(0.3)Au(0.7) catalysts, indicating that they are not able to break the C-C bond. The formation of hydroxypyruvate ion, which is a costly chemical product, is detected on pure gold catalyst