Dissemin is shutting down on January 1st, 2025

Published in

Wiley, Journal of Biomedical Materials Research Part B: Applied Biomaterials, 1(96B), p. 84-90, 2010

DOI: 10.1002/jbm.b.31742

Links

Tools

Export citation

Search in Google Scholar

Control of magnesium corrosion and biocompatibility with biomimetic coatings

Journal article published in 2010 by Sigrid Keim, Johannes G. Brunner, Ben Fabry ORCID, Sannakaisa Virtanen
This paper was not found in any repository, but could be made available legally by the author.
This paper was not found in any repository, but could be made available legally by the author.

Full text: Unavailable

Green circle
Preprint: archiving allowed
Orange circle
Postprint: archiving restricted
Red circle
Published version: archiving forbidden
Data provided by SHERPA/RoMEO

Abstract

The use of magnesium and its alloys as biodegradable metallic implant materials requires that their corrosion behavior can be controlled. We tailored the Mg release kinetics and cell adhesion properties of commercially pure Mg by chemical surface treatments in simulated body fluid, in Dulbecco's Modified Eagle's cell culture medium in the presence or absence of fetal bovine serum (FBS), or in 100% FBS. HeLa cells were cultured for 24 h on these Mg surfaces to characterize their biocompatibility. Cell density on all treated surfaces was significantly increased compared with a polished Mg surface, where almost no cells survived. This low biocompatibility of pure Mg was not caused by the high Mg ion release with concentrations of up to 300 mg/L in the cell culture medium after 24 h, as cells grown on a glass substrate showed no adverse reactions to high Mg ion concentrations. Rather, the most critical factor for cell adhesion was a sufficiently reduced initial dissolution rate of the surface. A comparison among all surface treatments showed that an incubation of the Mg samples in cell culture medium gave the lowest dissolution rate and resulted in the best cell adhesion and spreading behavior.