Elsevier, Thermochimica Acta, (561), p. 14-18
DOI: 10.1016/j.tca.2013.03.019
Export citation
Search in Google Scholar
Full text: Unavailable
Hydrogen desorption from R2Fe17Hx, (R=Nd and Dy) compounds with x