Published in

Journal of Biomedical Materials Research, 4(59), p. 709-715

DOI: 10.1002/jbm.10045

Links

Tools

Export citation

Search in Google Scholar

Bonelike Apatite Growth on Hydroxyapatite-Gelatin Sponges from Simulated Body Fluid

Journal article published in 2001 by A. Bigi, E. Boanini ORCID, S. Panzavolta, N. Roveri, K. J. Rubini
Distributing this paper is prohibited by the publisher
Distributing this paper is prohibited by the publisher

Full text: Unavailable

Red circle
Preprint: archiving forbidden
Orange circle
Postprint: archiving restricted
Red circle
Published version: archiving forbidden
Data provided by SHERPA/RoMEO

Abstract

In vitro bioactivity of gelatin sponges and hydroxyapatite-enriched gelatin sponges was tested through evaluation of the variations in their composition and morphology after soaking in simulated body fluid (1.5) for periods up to 21 days at 37 degrees C. The presence of hydroxyapatite inside the sponges promotes the deposition of bonelike apatite crystals. The deposits are laid down as spherical aggregates, with mean diameters increasing from about 1-2 microm, after 4 days of soaking in simulated body fluid solution, up to about 3.5 microm in the samples soaked for 21 days. Simultaneously, the relative amount of inorganic phase increases up to about 56% wt, leading to a composite material with a composition quite close to that of bone tissue. The inorganic phase is a poor crystalline carbonated apatite similar to trabecular bone apatite.