Evaluation of mechanical and thermal properties after chemical degradation of PVC and HDPE geomembranes

This paper is available in a repository.
This paper is available in a repository.

Full text: Download

Question mark in circle
Preprint: policy unknown
Question mark in circle
Postprint: policy unknown
Question mark in circle
Published version: policy unknown

Abstract

Chemical compatibility between geomembranes and site-specific waste liquids should be assessed since the waste liquids are highly complex mixtures. This paper presents some considerations about the chemical compatibility of geomembranes and some results of mechanical tests in HDPE and PVC geomembranes that were exposed to leachate and chemical residue (niobium). PVC and HDPE geomembranes of two thicknesses were tested: 1.0, 2.0 mm (PVC) and 0.8, 2.5 mm (HDPE). The results obtained show that after exposure the PVC geomembranes (1.0, 2.0 mm) were more rigid and stiffer than fresh samples. The HDPE geomembranes, on the other hand, when exposed to leachate and niobium residue presented increases in deformation. Melt flow index (MFI) tests were also carried out to verify the oxidation. © 2013 ejge.