Aqueous CSD of ferroelectric Bi3.5La0.5Ti3O12 (BLT) thin films

This paper was not found in any repository, but could be made available legally by the author.
This paper was not found in any repository, but could be made available legally by the author.

Full text: Unavailable

Red circle
Preprint: archiving forbidden
Orange circle
Postprint: archiving restricted
Red circle
Published version: archiving forbidden
Data provided by SHERPA/RoMEO

Abstract

A new, environmentally friendly, aqueous chemical solution deposition (CSD) route for the fabrication of BLT thin films is presented. Well crystallized, preferentially c-axis oriented films were obtained at 650degreesC. The grain size and remanent polarization were increased by the addition of an excess of Bi3+ to the precursor solution. At 10% Bi excess a P-r of 6.2 muC/cm(2) and E-c of 105 kV/cm were obtained.