Royal Society of Chemistry, Materials Advances, 4(2), p. 1294-1301, 2021
DOI: 10.1039/d0ma00955e
Full text: Unavailable
AIM-X catalysts were successfully obtained by depositing MoS2 within NU-1000 through ALD. The conversion rate of the obtained AIM-60 is much better than that of the traditional MoS2/γ-Al2O3, and it can directly convert dibenzothiophene to biphenyl.