Published in

MDPI, Materials, 24(12), p. 4196, 2019

DOI: 10.3390/ma12244196

Links

Tools

Export citation

Search in Google Scholar

Enamel Surface Roughness after Lingual Bracket Debonding: An In Vitro Study

This paper is made freely available by the publisher.
This paper is made freely available by the publisher.

Full text: Download

Green circle
Preprint: archiving allowed
Green circle
Postprint: archiving allowed
Green circle
Published version: archiving allowed
Data provided by SHERPA/RoMEO

Abstract

The aim of the present study was to quantitatively assess changes in enamel roughness parameters before and after lingual bracket debonding. The lingual surface of 25 sound premolars extracted for orthodontic reasons was studied by 3D optical interferometric profilometry before and after debonding of lingual brackets following enamel finishing (with fine diamond) and polishing (with 12- and 20-fluted carbide burs). The roughness parameters tested were the amplitude parameters Sa and Sz, the hybrid parameter Sdr, and the functional parameters Sc and Sv. The parameter differences (after debonding-reference) were calculated, and statistical analysis was performed via a Wilcoxon signed-rank test. Statistically significantly higher values were observed in all the surface roughness parameters of enamel surfaces after finishing and polishing, with the mostly affected parameter being the Sdr. Under the conditions of the present study, the finishing and polishing instruments used after debonding of lingual noncustomized brackets created a surface texture rougher than the control in all the tested roughness parameters.