Wiley, Angewandte Chemie International Edition, 42(52), p. 11119-11123, 2013
Wiley, Angewandte Chemie, 42(125), p. 11325-11329, 2013
Full text: Download
Covered with Pt: A uniform catalyst profile that ensures effective radial charge collection from high-aspect-ratio Si nanowires was achieved by atomic layer deposition of Pt nanoparticles. The resulting photoelectrode permits the measurement of high photovoltages and low overpotentials, and leads to very good stability against photooxidation of Si nanowires in solar water-reduction reactions.